Atomic Simulation of Nanoindentation on the Regular Wrinkled Graphene Sheet

Materials
Ruonan WangLianfeng Lai

Abstract

Surface landscapes have vague impact on the mechanical properties of graphene. In this paper, single-layered graphene sheets (SLGS) with regular wrinkles were first constructed by applying shear deformation using molecular dynamics (MD) simulations and then indented to extract their mechanical properties. The influence of the boundary condition of SLGS were considered. The wrinkle features and wrinkle formation processes of SLGS were found to be significantly related to the boundary conditions as well as the applied shear displacement and velocity. The wrinkling amplitude and degree of wrinkling increased with the increase in the applied shear displacements, and the trends of wrinkling wavelengths changed with the different boundary conditions. With the fixed boundary condition, the degree of graphene wrinkling was only affected when the velocity was greater than a certain value. The effect of wrinkles on the mechanical characterization of SLGS by atomic force microscopy (AFM) nanoindentation was finally investigated. The regular surface wrinkling of SLGS was found to weaken the Young's modulus of graphene. The Young's modulus of graphene deteriorates with the increase in the degree of regular wrinkling.

References

Oct 23, 2004·Science·K S NovoselovA A Firsov
Jul 20, 2005·Proceedings of the National Academy of Sciences of the United States of America·K S NovoselovA K Geim
Jan 27, 2007·Science·J Scott BunchPaul L McEuen
Mar 3, 2007·Nature·Jannik C MeyerS Roth
Jul 31, 2007·Nature Materials·F SchedinK S Novoselov
Sep 8, 2009·Nature Nanotechnology·Wenzhong BaoChun Ning Lau
Mar 11, 2010·Advanced Materials·Chang LiuHui-Ming Cheng
Mar 11, 2011·Journal of Physics. Condensed Matter : an Institute of Physics Journal·A J GilJ Bonet
May 3, 2011·Nano Letters·Carlos S Ruiz-VargasJiwoong Park
Nov 19, 2011·Nature·Kinam KimHyun-Jong Chung
Apr 16, 2013·Nanoscale·Changguo WangHuifeng Tan
Feb 1, 2015·Journal of Molecular Modeling·Jianzhang Huang, Qiang Han

❮ Previous
Next ❯

Methods Mentioned

BETA
atomic force microscopy
AFM

Software Mentioned

Large
OVITO
Scale Atomic / Molecular Massively Parallel Simulator ( LAMMPS )

Related Concepts

Trending Feeds

COVID-19

Coronaviruses encompass a large family of viruses that cause the common cold as well as more serious diseases, such as the ongoing outbreak of coronavirus disease 2019 (COVID-19; formally known as 2019-nCoV). Coronaviruses can spread from animals to humans; symptoms include fever, cough, shortness of breath, and breathing difficulties; in more severe cases, infection can lead to death. This feed covers recent research on COVID-19.

Blastomycosis

Blastomycosis fungal infections spread through inhaling Blastomyces dermatitidis spores. Discover the latest research on blastomycosis fungal infections here.

Nuclear Pore Complex in ALS/FTD

Alterations in nucleocytoplasmic transport, controlled by the nuclear pore complex, may be involved in the pathomechanism underlying multiple neurodegenerative diseases including Amyotrophic Lateral Sclerosis and Frontotemporal Dementia. Here is the latest research on the nuclear pore complex in ALS and FTD.

Applications of Molecular Barcoding

The concept of molecular barcoding is that each original DNA or RNA molecule is attached to a unique sequence barcode. Sequence reads having different barcodes represent different original molecules, while sequence reads having the same barcode are results of PCR duplication from one original molecule. Discover the latest research on molecular barcoding here.

Chronic Fatigue Syndrome

Chronic fatigue syndrome is a disease characterized by unexplained disabling fatigue; the pathology of which is incompletely understood. Discover the latest research on chronic fatigue syndrome here.

Evolution of Pluripotency

Pluripotency refers to the ability of a cell to develop into three primary germ cell layers of the embryo. This feed focuses on the mechanisms that underlie the evolution of pluripotency. Here is the latest research.

Position Effect Variegation

Position Effect Variagation occurs when a gene is inactivated due to its positioning near heterochromatic regions within a chromosome. Discover the latest research on Position Effect Variagation here.

STING Receptor Agonists

Stimulator of IFN genes (STING) are a group of transmembrane proteins that are involved in the induction of type I interferon that is important in the innate immune response. The stimulation of STING has been an active area of research in the treatment of cancer and infectious diseases. Here is the latest research on STING receptor agonists.

Microbicide

Microbicides are products that can be applied to vaginal or rectal mucosal surfaces with the goal of preventing, or at least significantly reducing, the transmission of sexually transmitted infections. Here is the latest research on microbicides.