Kinking nonlinear elastic solids, nanoindentations, and geology

Physical Review Letters
M W BarsoumT Zhen

Abstract

The physical mechanism responsible for nonlinear elastic, hysteretic, and discrete memory response of nonlinear mesoscopic elastic solids has to date not been identified. We show, by nanoindenting mica single crystals, that this response is most likely due to the formation of dissipative and fully reversible, dislocation-based kink bands. We further claim that solids with high c/a ratios, which per force are plastically anisotropic, should deform by kinking, provided they do not twin. These kinking nonlinear elastic solids include layered ternary carbides, nitrides, oxides, and semiconductors, graphite, and the layered phases, such as mica, present in nonlinear mesoscopic elastic solids.

References

Apr 24, 1995·Physical Review Letters·R A GuyerG N Boitnott
Mar 4, 2003·Nature Materials·M W BarsoumA Murugaiah
Apr 12, 2003·Physical Review Letters·Alexei MoussatovBernard Castagnède

❮ Previous
Next ❯

Citations

Sep 20, 2016·Scientific Reports·Jacob GruberMichel W Barsoum
May 3, 2006·Journal of Physics. Condensed Matter : an Institute of Physics Journal·Denis MusicJochen M Schneider
Mar 24, 2005·Physical Review Letters·M W BarsoumS R Kalidindi
Nov 29, 2011·Journal of Physics. Condensed Matter : an Institute of Physics Journal·D JürgensM W Barsoum
May 16, 2007·Physical Review Letters·Zicheng PanChangfeng Chen

❮ Previous
Next ❯

Trending Feeds

COVID-19

Coronaviruses encompass a large family of viruses that cause the common cold as well as more serious diseases, such as the ongoing outbreak of coronavirus disease 2019 (COVID-19; formally known as 2019-nCoV). Coronaviruses can spread from animals to humans; symptoms include fever, cough, shortness of breath, and breathing difficulties; in more severe cases, infection can lead to death. This feed covers recent research on COVID-19.

Blastomycosis

Blastomycosis fungal infections spread through inhaling Blastomyces dermatitidis spores. Discover the latest research on blastomycosis fungal infections here.

Nuclear Pore Complex in ALS/FTD

Alterations in nucleocytoplasmic transport, controlled by the nuclear pore complex, may be involved in the pathomechanism underlying multiple neurodegenerative diseases including Amyotrophic Lateral Sclerosis and Frontotemporal Dementia. Here is the latest research on the nuclear pore complex in ALS and FTD.

Applications of Molecular Barcoding

The concept of molecular barcoding is that each original DNA or RNA molecule is attached to a unique sequence barcode. Sequence reads having different barcodes represent different original molecules, while sequence reads having the same barcode are results of PCR duplication from one original molecule. Discover the latest research on molecular barcoding here.

Chronic Fatigue Syndrome

Chronic fatigue syndrome is a disease characterized by unexplained disabling fatigue; the pathology of which is incompletely understood. Discover the latest research on chronic fatigue syndrome here.

Evolution of Pluripotency

Pluripotency refers to the ability of a cell to develop into three primary germ cell layers of the embryo. This feed focuses on the mechanisms that underlie the evolution of pluripotency. Here is the latest research.

Position Effect Variegation

Position Effect Variagation occurs when a gene is inactivated due to its positioning near heterochromatic regions within a chromosome. Discover the latest research on Position Effect Variagation here.

STING Receptor Agonists

Stimulator of IFN genes (STING) are a group of transmembrane proteins that are involved in the induction of type I interferon that is important in the innate immune response. The stimulation of STING has been an active area of research in the treatment of cancer and infectious diseases. Here is the latest research on STING receptor agonists.

Microbicide

Microbicides are products that can be applied to vaginal or rectal mucosal surfaces with the goal of preventing, or at least significantly reducing, the transmission of sexually transmitted infections. Here is the latest research on microbicides.